Precision. Innovation. Tools.

Z=4 Torus Radius End Mill for Titanium

Z=4 torus radius end mill, developed to optimize tool life when machining titanium and its alloys.

The geometric configuration ensures high working stability, drastically reducing vibrations and preserving cutting-edge integrity even under demanding operating conditions.

The multilayer PVD Zirconium (Cer-Ni) coating acts as a thermal barrier, guaranteeing maximum resistance to high temperatures and effectively countering premature wear and material adhesion.

Code: 641
Code: 641
Suitable for
S
Titanium Alloys
DC
reset
3
4
5
6
8
10
12
16
20
OAL / L1
reset
57
63
72
83
92
104
APMX / L2
reset
8
11
13
19
22
26
32
38
Item codeTypeDCOAL / L1DCON / D2APMX / L2LHDNR / RE
641.030060857R030Ncoated3.0057.006.008.0012.002.900.30
641.040061157R030Ncoated4.0057.006.0011.0015.003.800.30
641.050061357R030Ncoated5.0057.006.0013.0017.004.800.30
641.060061357R050Ncoated6.0057.006.0013.0019.005.800.50
641.060061357R100Ncoated6.0057.006.0013.0019.005.801.00
641.060061357R150Ncoated6.0057.006.0013.0019.005.801.50
641.080081963R050Ncoated8.0063.008.0019.0025.007.700.50
641.080081963R100Ncoated8.0063.008.0019.0025.007.701.00
641.080081963R150Ncoated8.0063.008.0019.008.007.701.50
641.100102272R050Ncoated10.0072.0010.0022.0030.009.700.50
641.100102272R100Ncoated10.0072.0010.0022.0030.009.701.00
641.100102272R150Ncoated10.0072.0010.0022.008.009.701.50
641.120122683R100Ncoated12.0083.0012.0026.0034.0011.501.00
641.120122683R200Ncoated12.0083.0012.0026.0034.0011.502.00
641.120122683R300Ncoated12.0083.0012.0026.0034.0011.503.00
641.160163292R100Ncoated16.0092.0016.0032.0047.0015.501.00
641.160163292R200Ncoated16.0092.0016.0032.0047.0015.502.00
641.160163292R400Ncoated16.0092.0016.0032.0047.0015.504.00
641.2002038104R200Ncoated20.00104.0020.0038.0053.0019.502.00
641.2002038104R300Ncoated20.00104.0020.0038.0053.0019.503.00
641.2002038104R500Ncoated20.00104.0020.0038.0053.0019.505.00

Tolleranze / Tolerances

DC h10
APMX 0/+2
OAL 0/+2
LH 0/+2
DCON h6
RE 0/-0,04
DN 0/-0,05

 

Parametri di Lavoro / Working Parameters

Information on cookies on this site

This site uses anonymous technical and statistical cookies, necessary for its operation.

Read more x
0
Prod.